posted 13 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 112,
Visits: 1K
Would styrene work good as a thinner for GC50?
Mine is getting a bit old and starts to gel a little, not possible to spray anymore.
http://motoform.blogspot.se
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Styrene as thinner for GC50?
prsw
-
13 Years Ago
The reason it's gelling is partly because some styrene has evaporated but also because some cross...
carboncactus
-
13 Years Ago
Thanks Cactus
prsw
-
13 Years Ago
I thin resins by standing the main pot in an outer pot of boiling water. Works a treat!
FLD
-
13 Years Ago
[quote][b]FLD (21/06/2013)[/b][hr]I thin resins by standing the main pot in an outer pot of boiling...
prsw
-
13 Years Ago
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search