By prsw - 6/19/2013 7:12:44 PM

Would styrene work good as a thinner for GC50?

Mine is getting a bit old and starts to gel a little, not possible to spray anymore.
By prsw - 7/5/2013 8:32:29 AM

FLD (21/06/2013)
I thin resins by standing the main pot in an outer pot of boiling water.  Works a treat!


Thanks, how much does the heat shorten the geltime?
Do you use less mekp?