posted 13 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 7,
Visits: 42
I need some help, I just recieved my first order of prepreg and after playing with it for the last couple days I am horribly disappointed. I have been working with other prepregs from another supplier and I have had pretty good success with conventional prepreg that is meant to be cured in an autoclave even though I have been using it in an out of autoclave process. So far the first 5 things I have tried to make with easy preg have all been complete failures. I am super frustrated because I spent a lot of money to buy a couple yards of the material and have it sent to the US and at this point I am feeling like it all needs to be thrown in the trashcan because it seems completely useless. I will describe the setup that I am using and maybe someone can tell me what I might be doing wrong. I will also attach some pictures of the problems I am having. I have tried metal molds, composite molds with a gelcoat surface, cnc machined solid teflon molds, and tonight even a sheet of glass to see if I could get a good surface finish and so far all have failed miserably. For my mold release I am using a chemical release called Freekote 700nc which has performed beautifully with the other prepregs I have used. I am vacuum bagging with a flexible bagging material called stretchlon 200 and with a solid release film and a breather cloth. I have used cure schedules all over the map from 180 deg F for ten hours up to 275 deg F for less than an hour and all have yielded similar results The max amount of vac I am able to achieve here is about 26.5inches of mercury and that has proven to be acceptable for the other prepreg I have used but I am wondering if it is not enough for the easy preg because I have read a couple of places that a near perfect vac level above 29 inches is necessary. I leave the vac pump running throughout the process every time. To top it all off I am not at all happy with how the cured fiber looks and find it to be some of the most boring carbon fiber I have ever seen anywhere. There seems to be such a lack of contrast of the alternating fibers that it almost doesn't even look like carbon fiber at all, I would hope that if I could get my surface finish issues resolved the appearance might also improve but I am skeptical that it will ever look as good as any of the other various fabrics I have worked with. For me the selling point of this prepreg was that it was great for making cosmetic parts and I am disappointed to say the least. I appreciate any input that I can get and really hope that I am doing something wrong and that I can learn to love this easy preg! Thanks for your help.
The first two pictures show a piece that I cured on glass, It consists of one surfacing layers and two backing layers bagged up as I have described above. The last two pictures show some parts I have made with another brand of prepreg shown with the same piece molded on glass. The skull and the outlet cover do have automotive clear coat on them and although I realize that it may not seem like a fair comparison I can tell you that the clear coat does not hide any flaws, but if anything tends to magnify them.
Attachments
carbon1.jpg
(
1.1K views,
647.00 KB
)
carbon2.jpg
(
852 views,
847.00 KB
)
carbon3.jpg
(
1K views,
716.00 KB
)
carbon4.jpg
(
824 views,
645.00 KB
)
Reply
Like
6
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Terrible Surface finish-Please help!!c
nebraskatrevor
-
13 Years Ago
Hi Trev, I use a surfacing system from Umeco (VTF261). It seems identical to the easypreg surface...
carboncactus
-
13 Years Ago
Thanks so much for your reply. The results you achieve with your fender are exactly what i am after...
nebraskatrevor
-
13 Years Ago
At 400 metres, your maximum vac will be around -0.94 bar. Test both your vacuum and your gauge by...
carboncactus
-
13 Years Ago
Beautifull fender. PerhapsI have not been as careful as i need to be when bagging. I will try a...
nebraskatrevor
-
13 Years Ago
I'm sure you'll get there. Another helper is debulking. Once you've tested the bag and befoere you...
carboncactus
-
13 Years Ago
I went and purchased a new vac pump and gauge today (pic one) and refined my bagging methods some...
nebraskatrevor
-
13 Years Ago
[quote][b]nebraskatrevor (16/06/2013)[/b][hr]I went and purchased a new vac pump and gauge today...
fgayford
-
13 Years Ago
Again, I can't talk about easypreg, only the Umeco product I use. When you say "cosmetic" do you...
carboncactus
-
13 Years Ago
You are right me saying it looks better is just a matter of opinion but I want my carbon fiber to...
nebraskatrevor
-
13 Years Ago
Did you still just whack it straight in the preheated oven? Did you mix and match pumps and gauges...
carboncactus
-
13 Years Ago
I did mess aouund with pumps and gauges and the results I achieved were with the new pump and new...
nebraskatrevor
-
13 Years Ago
I'll let someone from EC tell me otherwise, but I think you'll find the surface layer cures between...
carboncactus
-
13 Years Ago
Looks like not enough vacuum or heated up too quickly or poor bagging. In terms of "depth and...
Warren (Staff)
-
13 Years Ago
Like Carbon Cactus I use VTF261 and get flawless parts from OOA carbon. I just think it is care and...
morepower
-
13 Years Ago
Good to see you here, morepower! :) Heres some photos of the most common leaks I get, they are...
carboncactus
-
13 Years Ago
[quote][b]carboncactus (17/06/2013)[/b][hr]Good to see you here, morepower! :) Heres some photos...
fgayford
-
13 Years Ago
Thought I would take a look round.... I might need to look at how surf boards are made... Haha.......
morepower
-
13 Years Ago
[quote][b]morepower (17/06/2013)[/b][hr]Thought I would take a look round.... I might need to look...
fgayford
-
13 Years Ago
Thanks to all of the suggestions I have received here I am getting much closer to success with the...
nebraskatrevor
-
13 Years Ago
Thanks nebraskatrevor for the updates, I ve been following the entire post because I'll try prepreg...
matthieutje65
-
13 Years Ago
Glad to see the improvements, trev. Are you happier with the cosmetics of it? Clear coat and wax...
carboncactus
-
13 Years Ago
Post Reply
Like
6
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search