Just found out that there are apparently some incompatabilities with epoxy and polyester resin and that one cannot be laid over the other and visa versa.  Is that true?
I made a part with epoxy and then used some polyester body filler on it before putting some more epoxy in it which has not cured properly, I was wondering, could the body filler have affected the epoxy?