Group: Forum Members
Posts: 33,
Visits: 187
|
Just found out that there are apparently some incompatabilities with epoxy and polyester resin and that one cannot be laid over the other and visa versa. Is that true? I made a part with epoxy and then used some polyester body filler on it before putting some more epoxy in it which has not cured properly, I was wondering, could the body filler have affected the epoxy?
|