RESIN USED FOR CARBON FIBER Prepreg?????


Author
Message
Warren (Staff)
Warren (Staff)
Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
You dont "use" a resin with pre-preg. It comes pre-mixed and pre-applied to the carbon so there is no mix ratio for you to deal with.

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
liu
liu
Junior Member (23 reputation)Junior Member (23 reputation)Junior Member (23 reputation)Junior Member (23 reputation)Junior Member (23 reputation)Junior Member (23 reputation)Junior Member (23 reputation)Junior Member (23 reputation)Junior Member (23 reputation)
Group: Forum Members
Posts: 3, Visits: 21
May i Know what resin is used for carbon fiber prepreg. one part or two part resin. if two part what is the ratio for resin and hardener?

Thanksssssss!