May i Know what resin is used for carbon fiber prepreg. one part or two part resin. if two part what is the ratio for resin and hardener?
Thanksssssss!
|
By Warren (Staff) - 5/14/2013 3:16:51 PM
You dont "use" a resin with pre-preg. It comes pre-mixed and pre-applied to the carbon so there is no mix ratio for you to deal with.
|
|