Exocet
Exocet
posted 13 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 12,
Visits: 119
Warren (Staff) (05/04/2013)
Your plan seems sound to me. Just be extra careful that the filler isnt pourous and is sealed before release coating. You dont want the part sticking.
Warren, thanks for your reply. One last question, in terms of sealing the filler what would you recommend. I'm using an automotive stopper for the filler so i guess its cellulose based.
Thanks
John
Reply
Like
5
Warren (Staff)
Warren (Staff)
posted 13 Years Ago
ANSWER
HOT
Post Details
Group: Administrators
Posts: 2.5K,
Visits: 8.5K
Your plan seems sound to me. Just be extra careful that the filler isnt pourous and is sealed before release coating. You dont want the part sticking.
We would recommend our
EL2 Epoxy Laminating Resin
for the general laminating.
In terms of gelcoat I would recommend our
GC50 Epoxy Compatible Polyester Gelcoat
as it can be brushed on with care and offers significant UV protection which may be useful for your dashboard.
3 layers would be fairly flexible in the middle but stiff as hell at the bottom due to the curved lip. 4 layers would stiffen it up nicely. As its cosmetic you could use a woven glass for the backing layers to save costs.
Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
Tags
dash
Reply
Like
5
Exocet
Exocet
posted 13 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 12,
Visits: 119
Hi, Firstly just found this forum, what a great resource. So I have the following questions I would really welcome any advice on.
THE PROJECT - a simple carbon fibre dashboard, consists of a flat plat 6" wide with a 11/2" radius along one edge. Wet layed.
THE MOULD - I've use a simple sheet of 'Conti' board (chipboard with a white laminated surface) with half a plastic pipe to form the radius. This has be filled and flatted down with 800 Grit wet and dry, I will flat the whole mould with 1200 grit next. I attached a photo for reference.
QUESTIONS/ ADVICE
1) I plan to use Easy lease release agent followed by two coats of release wax, is this ok?
2) As I'm wet laying what Gel coat and resin system do you recommend?
4) I plan on mixing gently with a hairdryer on hand to help remove any bubbles in the gel coat.
5) Was planning of using 'Pro Finish 2/2 twill carbon fibre (to help perserve the look of the fibre and cutting would be easier), would 3 sheets be sufficent, its not structure?
6) Bristle roller.
Have I missed anything else ? Thanks in advance - this will be my first time working with Carbon however I have laminated G/F before.
Tags
carbon
dash board.
wet lay
Reply
Like
6
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Post Reply
Like
6
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search