Thank you Matthieu,
Your idea is very good, and I think it would be very strong done like that...
To say the through I think it would not be so easy to layup the alraeady casted mounting points in the main piece, and almost impossible if you do it with infusion.
I think I will try to glue it somehow on the main piece
You say you need casting resin... do you think laminating resin or infusion resion would not be good just for litte parts like these? What is the differebce from casting resin to the pther kind?
I don't have casting resin and I'd need to buy it just for this... so if i can do without...