dont be afraid to experiment when making mold reinforcements
dont be afraid to experiment when making mold reinforcements
Post Reply
Like
3
dont be afraid to experiment when making mold reinforcements
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
Vips
Vips
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 13,
Visits: 381
Be careful with airborne Talc when mixing. A P3 filtered mask is a must.
Reply
Like
2
brasco
brasco
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 192,
Visits: 305
outstanding guys !! thanks for teh info and the posts
CarbonFiberCreations
Reply
Like
3
FLD
FLD
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 468,
Visits: 2.7K
These are old skool methods. I use wood in all my big moulds to reinforce them. You can get paper rope with wire in it which is good for adding stiffening ribs too.
Reply
Like
3
neilb
neilb
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 107,
Visits: 504
have been using talc for a while its good stuff!
Reply
Like
2
wozza
wozza
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 688,
Visits: 5.4K
Garden hose cut to length and glassed onto the back of moulds make great stiffeners/reinforcement. It follows curves and is quick and easy to apply.
Warren
Carbon
Copies Ltd
Edited
12 Years Ago by
wozza
Reply
Like
3
brasco
brasco
posted 12 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 192,
Visits: 305
very interesting. i liked how they seem to have the wood pieces all planned and ready, like this is how their usual molds are done.
and using talc and resin mixed up as a stiffening medium i thought was a good idea as well.
CarbonFiberCreations
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search