I have to say EC staff is very concerned about customer service. i had a minor problem with gum tape (two rolls hardly stuck together, thus loosing a few meters during separating them) and issues with an OLD MODEL of resin catch pot, WHICH IS NOT FOR SALE ANYMORE in case you wonder.

They replaced the two rolls of gum tape, and now they separate rolls with non stick sheet, so even under pressure during transport, rolls dont stick together anymore.

For the resin catch pot, since I made a new one with my little fingers, they proposed me to "replace it" with equivalent value of other products i would need.

Those guys rock, which is not often the case when you order stuff online from another country than yours.

Cheers from Belgium.

 



 


    A $1000 electronic device will always protect a 10 cents fuse
Zekewarg
Zekewarg
Supreme Being (362 reputation)Supreme Being (362 reputation)Supreme Being (362 reputation)Supreme Being (362 reputation)Supreme Being (362 reputation)Supreme Being (362 reputation)Supreme Being (362 reputation)Supreme Being (362 reputation)Supreme Being (362 reputation)
Group: Forum Members
Posts: 42, Visits: 241
Thanks! Smile
Paul (Staff)
Paul (Staff)
Technical Support (1.4K reputation)Technical Support (1.4K reputation)Technical Support (1.4K reputation)Technical Support (1.4K reputation)Technical Support (1.4K reputation)Technical Support (1.4K reputation)Technical Support (1.4K reputation)Technical Support (1.4K reputation)Technical Support (1.4K reputation)
Group: Administrators
Posts: 134, Visits: 614
Hi Zach,

You are doing nothing wrong... That's what it displays if it has been overloaded, it must have taken a big knock in transit. Sorry for the inconvienience, we'll get another set sent straight out to you.

Paul Statham
Easy Composites / Carbon Mods - Technical
Zekewarg
Zekewarg
Supreme Being (362 reputation)Supreme Being (362 reputation)Supreme Being (362 reputation)Supreme Being (362 reputation)Supreme Being (362 reputation)Supreme Being (362 reputation)Supreme Being (362 reputation)Supreme Being (362 reputation)Supreme Being (362 reputation)
Group: Forum Members
Posts: 42, Visits: 241
Hi guys.

Just unwrapped the digital scale that came with the shipment yesterday.
But when I turn it on it only reads "Out 2".
Have tried pressing everything and loading the scale but nothing happens?
What am I doing wrong?

Cheers Zach
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search