Hi guys.
Just unwrapped the digital scale that came with the shipment yesterday.
But when I turn it on it only reads "Out 2".
Have tried pressing everything and loading the scale but nothing happens?
What am I doing wrong?
Cheers Zach
By Joe
-
2/2/2012 6:35:42 PM
I have to say EC staff is very concerned about customer service. i had a minor problem with gum tape (two rolls hardly stuck together, thus loosing a few meters during separating them) and issues with an
OLD MODEL
of resin catch pot,
WHICH IS NOT FOR SALE ANYMORE
in case you wonder.
They replaced the two rolls of gum tape, and now they separate rolls with non stick sheet, so even under pressure during transport, rolls dont stick together anymore.
For the resin catch pot, since I made a new one with my little fingers, they proposed me to "replace it" with equivalent value of other products i would need.
Those guys rock, which is not often the case when you order stuff online from another country than yours.