I need to start using a mould asap after mould-making, would one day with watersanding/polishing  and waxing be enough?
I am thinking about the solvents etc in the gelcoat, whats your recommended time to let them "de-gas"?


http://motoform.blogspot.se

Warren (Staff)
Warren (Staff)
Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
We always recommend a postcure with the Uni-Mould system, however if that isnt possible, 48 hours wait should be fine before you start polishing and sanding it.

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
Matthieu Libeert
Matthieu Libeert
Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)
Group: Forum Members
Posts: 955, Visits: 3.4K
What resin did you use for the mouldmaking? Polyester or epoxy or vinylester?

Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com




prsw
prsw
Supreme Being (904 reputation)Supreme Being (904 reputation)Supreme Being (904 reputation)Supreme Being (904 reputation)Supreme Being (904 reputation)Supreme Being (904 reputation)Supreme Being (904 reputation)Supreme Being (904 reputation)Supreme Being (904 reputation)
Group: Forum Members
Posts: 112, Visits: 1K
I post cured it today, it will get time needed.
Thx


http://motoform.blogspot.se

GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search