By prsw - 2/12/2013 6:34:42 AM
I need to start using a mould asap after mould-making, would one day with watersanding/polishing and waxing be enough? I am thinking about the solvents etc in the gelcoat, whats your recommended time to let them "de-gas"?
|
By prsw - 2/12/2013 10:13:31 PM
I post cured it today, it will get time needed. Thx
|
|