Closed cell foam sandwich construction


Author
Message
Gerrit
Gerrit
Forum Member (49 reputation)Forum Member (49 reputation)Forum Member (49 reputation)Forum Member (49 reputation)Forum Member (49 reputation)Forum Member (49 reputation)Forum Member (49 reputation)Forum Member (49 reputation)Forum Member (49 reputation)
Group: Forum Members
Posts: 3, Visits: 7
Hi,

Is it possible to make sandwich panels using closed cell foam and pre-preg carbon fiber flat sheet? If so, what kind of adhesive would be required?
I would like to create a sandwich panel using 3mm thick foam and 0.25mm or 0.5mm sheet.



Kind regards,

Gerrit
Reply
Warren (Staff)
Warren (Staff)
Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
Cool! glad it worked!  one of our staff members made a similar panel using some Nomex honeycomb to reduce the weight even further for bulkheads in his RC plane.

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search