Gerrit
Gerrit
posted 13 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 3,
Visits: 7
Hi,
Is it possible to make sandwich panels using closed cell foam and pre-preg carbon fiber flat sheet? If so, what kind of adhesive would be required?
I would like to create a sandwich panel using 3mm thick foam and 0.25mm or 0.5mm sheet.
Kind regards,
Gerrit
Reply
Like
8
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Closed cell foam sandwich construction
Gerrit
-
13 Years Ago
Hi Gerrit We recommend using our ET538Honeycomb Bonding Epoxy Adhesive Normal...
Warren (Staff)
-
13 Years Ago
Hi Warren, Thanks for the speedy reply and advice. I just placed an order for some materials to...
Gerrit
-
13 Years Ago
Let us know how you get on.
Warren (Staff)
-
13 Years Ago
Hi Warren, It worked like a charm. It's truly amazing how strong the panel becomes once the second...
Gerrit
-
13 Years Ago
Cool! glad it worked! one of our staff members made a similar panel using some Nomex honeycomb to...
Warren (Staff)
-
13 Years Ago
Post Reply
Like
8
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search