By Gerrit - 1/28/2013 10:14:19 AM

Hi,

Is it possible to make sandwich panels using closed cell foam and pre-preg carbon fiber flat sheet? If so, what kind of adhesive would be required?
I would like to create a sandwich panel using 3mm thick foam and 0.25mm or 0.5mm sheet.



Kind regards,

Gerrit
By Warren (Staff) - 2/20/2013 3:37:17 PM

Cool! glad it worked!  one of our staff members made a similar panel using some Nomex honeycomb to reduce the weight even further for bulkheads in his RC plane.