Composite tubes with infusion


Author
Message
Raf4C
R
posted Last Year HOT
Supreme Being (179 reputation)Supreme Being (179 reputation)Supreme Being (179 reputation)Supreme Being (179 reputation)Supreme Being (179 reputation)Supreme Being (179 reputation)Supreme Being (179 reputation)Supreme Being (179 reputation)Supreme Being (179 reputation)
Group: Forum Members
Posts: 12, Visits: 86
Dear All,

I could not find any relevant information on this topic, which is why I am reaching out for advice.

I am attempting to infuse composite tubes and have 3D-printed a mold using a soluble polymer to facilitate easy removal at the end of the process. I have also developed a method to keep the fibers (tested with both glass and carbon) tightly positioned during the infusion. Additionally, I have found a way to secure the peel ply and the vacuum bag effectively.

However, I am encountering an issue: when applying vacuum, wrinkles form in the bag due to the multiple turns of the fibers, as I am trying to create a multi-layered tube.

Has anyone faced a similar challenge or has any suggestions on how to mitigate this problem?

Best regards,
Raf