Here is a pic of my first part. Not terrible but not useable. I think the biggest problem with the part being useable was the fact that I tried to take it out too soon.

I think the biggest issue I am having is putting the bagging material with pleats on the molds. I have no problems getting the bags to seal I just need to learn how to get the bag to finish nicely at the last corner or down the last side. I always seem to have not enough bag to put the size pleat I wanted to or I get to the last bit and I have too much bag left over and I can't get the bag to lay flat with out a mini pleat. It is real frustrating and hard to deal with since at this point you dont have alot of maneuverability.

Any sugestions?

Thanks,  Dennis
Edited 13 Years Ago by Dennis G