Group: Forum Members
Posts: 34,
Visits: 837
|
Thanks for the replies, I did remake this part and it came out much better but still not perfect. I think the second one will be useable once it is trimmed 98% of any issues will be gone. The biggest issue with this part is around the tight radius on the outside of the raised area in the middle. I cant seem to get the CF to fit tight to the mold. Actually I think the issue is with the infusion mesh. The mesh doesn't seem to contour very nicely. Should I be cutting this into multiple pieces? Any tips for the infusion mesh?