New high temp vinylester mould making pva problems.


Author
Message
kip
kip
kip
posted 5 Years Ago HOT
Supreme Being (462 reputation)Supreme Being (462 reputation)Supreme Being (462 reputation)Supreme Being (462 reputation)Supreme Being (462 reputation)Supreme Being (462 reputation)Supreme Being (462 reputation)Supreme Being (462 reputation)Supreme Being (462 reputation)
Group: Forum Members
Posts: 32, Visits: 99
I got some weird problems I never had before in all my vinylester moulds I made.
I'm now using a high temp 145°C vinylester mould system  and to be sure I get no release problems on the parts  carbon fibre winglets I used PVA

So I waxed mould 7 times with high temp wax and than used pva this all went well .
After the layup the release was verry good little to good even it almost fel off but  the problem is the high gloss clearcoated carbon winglets are full  little pinoles and the mould surface also .

after demoulding I stil could peal off the pva film from the  gelcoat side verry good .

I'm using  partal coverall pva purple one because this works with the  tr104 high temp wax



GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
kip - 5 Years Ago
Hanaldo - 5 Years Ago
kip - 5 Years Ago
Hanaldo - 5 Years Ago
kip - 5 Years Ago
Hanaldo - 5 Years Ago
kip - 5 Years Ago
Hanaldo - 5 Years Ago
kip - 5 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search