Oh, that's just a reaction between the gelcoat and the paint on the part. Quite normal when moulding off polyurethanes. They soften slightly and get a little bit attacked by the styrene. Not enough to cause an issue, but enough to haze both surfaces a little.
Mould will just need a cut and polish.
|