Split mould. Where to split?


Author
Message
Fasta
Fasta
Supreme Being (6.7K reputation)Supreme Being (6.7K reputation)Supreme Being (6.7K reputation)Supreme Being (6.7K reputation)Supreme Being (6.7K reputation)Supreme Being (6.7K reputation)Supreme Being (6.7K reputation)Supreme Being (6.7K reputation)Supreme Being (6.7K reputation)
Group: Forum Members
Posts: 468, Visits: 3.5K
Darren - 1/15/2021 6:27:41 PM
I don't think either of those ideas will work. There are returns front and rear, also the top of the head light recess has an 20mm return

Of course is hard to see all the details in pics.

Where there are return edges if needed these can be a separate bolt on flange which can allow release.
If needed the headlight bucket area could be a separate loose piece held into the moulds with fastenings?

I am sure there is a way, but try to keep the plan clean/simple and easy if possible.





Darren
Darren
Supreme Being (674 reputation)Supreme Being (674 reputation)Supreme Being (674 reputation)Supreme Being (674 reputation)Supreme Being (674 reputation)Supreme Being (674 reputation)Supreme Being (674 reputation)Supreme Being (674 reputation)Supreme Being (674 reputation)
Group: Forum Members
Posts: 54, Visits: 916
I don't think either of those ideas will work. There are returns front and rear, also the top of the head light recess has an 20mm return
Fasta
Fasta
Supreme Being (6.7K reputation)Supreme Being (6.7K reputation)Supreme Being (6.7K reputation)Supreme Being (6.7K reputation)Supreme Being (6.7K reputation)Supreme Being (6.7K reputation)Supreme Being (6.7K reputation)Supreme Being (6.7K reputation)Supreme Being (6.7K reputation)
Group: Forum Members
Posts: 468, Visits: 3.5K
Maybe the it could be one single split line right down the centre line except that it would need to be done without the that hole in the front (fill it up for making the mould) and then have a loose piece that screws into the assembled moulds to create the hole??

Or it could be split into three pieces with a split line down the top centre of the fenders/above the wheels and through or around the headlights?








Edited 5 Years Ago by Fasta
Darren
Darren
Supreme Being (674 reputation)Supreme Being (674 reputation)Supreme Being (674 reputation)Supreme Being (674 reputation)Supreme Being (674 reputation)Supreme Being (674 reputation)Supreme Being (674 reputation)Supreme Being (674 reputation)Supreme Being (674 reputation)
Group: Forum Members
Posts: 54, Visits: 916
Moulding the front end of a lotus 23b. 

Where would be the ideal spilt lines for the mould? 