Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Advanced Composites Forum
»
Mould Making
»
Split mould. Where to split?
Split mould. Where to split?
Post Reply
Like
7
Split mould. Where to split?
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
Darren
Darren
posted 5 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 54,
Visits: 916
Moulding the front end of a lotus 23b.
Where would be the ideal spilt lines for the mould?
Reply
Like
7
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Split mould. Where to split?
Darren
-
5 Years Ago
Maybe the it could be one single split line right down the centre line except that it would need to be done without the that hole in the front (fill it up for making the mould) and then have a loose....
Fasta
-
5 Years Ago
I don't think either of those ideas will work. There are returns front and rear, also the top of the head light recess has an 20mm return
Darren
-
5 Years Ago
Of course is hard to see all the details in pics. Where there are return edges if needed these can be a separate bolt on flange which can allow release. If needed the headlight bucket area could be ...
Fasta
-
5 Years Ago
Post Reply
Like
7
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search