Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Advanced Composites Forum
»
Resin Infusion
»
Bag shape
Bag shape
Post Reply
Like
4
Bag shape
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
Massimiliano
M
Massimiliano
posted 6 Years Ago
ANSWER
HOT
Topic Details
M
Group: Forum Members
Posts: 167,
Visits: 1.1K
Hello,
maybe a silly question but... for the mold below what shape would you recommend for the bag?
A big rectangle with of course more pleats on the shorter sides of the mold or try to make the bag similar shape of the mold (of course bigger to allow for pleats)?
Thanks
Reply
Like
4
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Bag shape
mporta71
-
6 Years Ago
Yeh I would just go with a big rectangle, its simpler. Cutting the bag to shape is good, but it means you have to get your pleat sizes spot on otherwise you dont position the bag correctly.
Hanaldo
-
6 Years Ago
Thank you!
mporta71
-
6 Years Ago
I agree with the big rectangle - maybe try orienting it along the bounding box of the mold. Lots of pleats. Also putting the sealant tape on the perimeter of the bag first will make it way easier and...
explorecomposites
-
6 Years Ago
Yes I see your videos and will do as you do, thank you!
mporta71
-
6 Years Ago
Post Reply
Like
4
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search