Chris Rogers - 12/26/2020 7:55:19 PM
I agree with the big rectangle - maybe try orienting it along the bounding box of the mold.  Lots of pleats. Also putting the sealant tape on the perimeter of the bag first will make it way easier and faster!  Forming pleats becomes quick and flexible and it only wastes a little sealant tape.  

Yes I see your videos and will do as you do, thank you!

Chris Rogers
C
Supreme Being (1.3K reputation)Supreme Being (1.3K reputation)Supreme Being (1.3K reputation)Supreme Being (1.3K reputation)Supreme Being (1.3K reputation)Supreme Being (1.3K reputation)Supreme Being (1.3K reputation)Supreme Being (1.3K reputation)Supreme Being (1.3K reputation)
Group: Forum Members
Posts: 120, Visits: 933
I agree with the big rectangle - maybe try orienting it along the bounding box of the mold.  Lots of pleats. Also putting the sealant tape on the perimeter of the bag first will make it way easier and faster!  Forming pleats becomes quick and flexible and it only wastes a little sealant tape.  




Massimiliano
M
Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)
Group: Forum Members
Posts: 167, Visits: 1.1K
Hanaldo - 12/26/2020 6:01:17 AM
Yeh I would just go with a big rectangle, its simpler. Cutting the bag to shape is good, but it means you have to get your pleat sizes spot on otherwise you dont position the bag correctly. 

Thank you!

Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
Yeh I would just go with a big rectangle, its simpler. Cutting the bag to shape is good, but it means you have to get your pleat sizes spot on otherwise you dont position the bag correctly. 
Massimiliano
M
Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)
Group: Forum Members
Posts: 167, Visits: 1.1K
Hello,
maybe a silly question but... for the mold below what shape would you recommend for the bag?
A big rectangle with of course more pleats on the shorter sides of the mold or try to make the bag similar shape of the mold (of course bigger to allow for pleats)?
Thanks



GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search