Thx,

I use Adobe Aftereffects and the written part is with a wacom in photoshop Smile

Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com




Jack.Strong
Jack.Strong
Supreme Being (354 reputation)Supreme Being (354 reputation)Supreme Being (354 reputation)Supreme Being (354 reputation)Supreme Being (354 reputation)Supreme Being (354 reputation)Supreme Being (354 reputation)Supreme Being (354 reputation)Supreme Being (354 reputation)
Group: Forum Members
Posts: 52, Visits: 549
Nice videos, pretty interesting!

What software are you using to have hand written text popup ?
Matthieu Libeert
Matthieu Libeert
Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)
Group: Forum Members
Posts: 955, Visits: 3.4K
Hi guys,

Just made a new 2-part tutorial video that might be interesting for some here on this forum.
It's about making Silicone mould and getting parts out of it.
By doing this you can duplicate parts and even make many more.

Ive used Silicone ZA 22 and Casting resin F18 Fastcast Polyurethane (Axson)
Easy composites sells similar products that you can buy on their website if interested.
Don't forget that different products have slightly different properties and mixing ratios!

Part 1: Silicone mouldmaking


Part 2: Casting parts out of mould


Kind regards,

Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com




GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search