Tutorial - Silicone mouldmaking and casting parts

http://www.talkcomposites.com/Topic3844.aspx

By matthieutje65 - 12/15/2012 8:19:28 PM

Hi guys,

Just made a new 2-part tutorial video that might be interesting for some here on this forum.
It's about making Silicone mould and getting parts out of it.
By doing this you can duplicate parts and even make many more.

Ive used Silicone ZA 22 and Casting resin F18 Fastcast Polyurethane (Axson)
Easy composites sells similar products that you can buy on their website if interested.
Don't forget that different products have slightly different properties and mixing ratios!

Part 1: Silicone mouldmaking


Part 2: Casting parts out of mould


Kind regards,
By matthieutje65 - 12/19/2012 2:32:35 AM

Thx,

I use Adobe Aftereffects and the written part is with a wacom in photoshop Smile