Matthieu Libeert
Matthieu Libeert
posted 13 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 955,
Visits: 3.4K
Hi guys,
Just made a new 2-part tutorial video that might be interesting for some here on this forum.
It's about making Silicone mould and getting parts out of it.
By doing this you can duplicate parts and even make many more.
Ive used Silicone ZA 22 and Casting resin F18 Fastcast Polyurethane (Axson)
Easy composites sells similar products that you can buy on their website if interested.
Don't forget that different products have slightly different properties and mixing ratios!
Part 1: Silicone mouldmaking
Part 2: Casting parts out of mould
Kind regards,
Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com
Reply
Like
2
Jack.Strong
Jack.Strong
posted 13 Years Ago
ANSWER
Post Details
Group: Forum Members
Posts: 52,
Visits: 549
Nice videos, pretty interesting!
What software are you using to have hand written text popup ?
Reply
Like
1
Matthieu Libeert
Matthieu Libeert
posted 13 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 955,
Visits: 3.4K
Thx,
I use Adobe Aftereffects and the written part is with a wacom in photoshop
Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com
Reply
Like
2
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Post Reply
Like
2
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search