Envelope vacuum bagging question


Author
Message
Massimiliano
M
Supreme Being (2.5K reputation)Supreme Being (2.5K reputation)Supreme Being (2.5K reputation)Supreme Being (2.5K reputation)Supreme Being (2.5K reputation)Supreme Being (2.5K reputation)Supreme Being (2.5K reputation)Supreme Being (2.5K reputation)Supreme Being (2.5K reputation)
Group: Forum Members
Posts: 167, Visits: 1.1K
Hi, for the mold I have it would be easier to use an envelope bag instead of a bag attached to the flange.
But how do you prevent resin running over the flange and filling the back breather cloth?