Massimiliano
M
Massimiliano
posted 5 Years Ago
ANSWER
HOT
Topic Details
M
Group: Forum Members
Posts: 167,
Visits: 1.1K
Hi, for the mold I have it would be easier to use an envelope bag instead of a bag attached to the flange.
But how do you prevent resin running over the flange and filling the back breather cloth?
Reply
Like
4
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Envelope vacuum bagging question
mporta71
-
5 Years Ago
You can't. One of the drawbacks of envelope bagging.
Hanaldo
-
5 Years Ago
So you apply release film on the back to avoid the breather become solid with the mold?
mporta71
-
5 Years Ago
If you intend to use the mould more than once then yes, this is generally best. Or skip the breather and just do several layers of peel ply. It is messy and can make using the mould a royal pain in.....
Hanaldo
-
5 Years Ago
Thank you!
mporta71
-
5 Years Ago
On moulds where I have needed to envelope bag regularly, I sanded the back of the mould smooth, then brushed on a thin layer of resin. Once cured I would Easy Lease coat it. That way any resin on the...
Warren (Staff)
-
5 Years Ago
Brilliant, thank you!
mporta71
-
5 Years Ago
Post Reply
Like
4
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search