gel coat thickness


Author
Message
ana
a
ana
posted 6 Years Ago HOT
Supreme Being (256 reputation)Supreme Being (256 reputation)Supreme Being (256 reputation)Supreme Being (256 reputation)Supreme Being (256 reputation)Supreme Being (256 reputation)Supreme Being (256 reputation)Supreme Being (256 reputation)Supreme Being (256 reputation)
Group: Forum Members
Posts: 14, Visits: 49
hi
please help me

I apply gel coat on the mold (
cast mold )
. but some area I applied more gel coat and these area  is thicker than another area ( some area has  mm gel coat and some area has 1.3mm gel coat. is it possible to different thickness effects on the
de-molding of my part from mold?
if yes, please let me know what is it exactly?

2- if i add more cobalt to polyester resin what is the effect of de-molding the part? is good or is not good?

tanks so much
Edited 6 Years Ago by ana