  I apply gel coat on the mold (cast mold )  . but some area I applied more gel coat and these area  is thicker than another area ( some area has  mm gel coat and some area has 1.3mm gel coat. is it possible to different thickness effects on the  de-molding of my part from mold? if yes, please let me know what is it exactly?
  2- if i add more cobalt to polyester resin what is the effect of de-molding the part? is good or is not good?
  tanks so much
           
		 | 			
		 
	
		
				      		    
		
		
            
            
            By Warren (Staff) - 10/13/2020 2:17:30 PM				
            
                      
            If its not coming out the mould, assuming release agent applied correctly, then it probably needs a bit more time to cure. Part cured or green resins tend to grip the mould and can be hard to demould.
           
		 | 			
		 
	
	
						
		 	
		
	 |