+x Lester Populaire - 9/7/2020 10:29:01 AM+x Massimiliano - 9/7/2020 9:36:15 AMHi, what is the recommended maximum fabric thickness for a one shot successful infusion, given a 250 cm2 square area?ThanksDepends in the fabric architecture and fibre type. I have done plates of 20mm thickness in one go without issue, and have done layups of 2mm in several steps to avoid problems with porosity.