Best fiber to reconstruct / repair


Author
Message
Zapan
Z
Junior Member (14 reputation)Junior Member (14 reputation)Junior Member (14 reputation)Junior Member (14 reputation)Junior Member (14 reputation)Junior Member (14 reputation)Junior Member (14 reputation)Junior Member (14 reputation)Junior Member (14 reputation)
Group: Forum Members
Posts: 1, Visits: 4
Hello.

Im looking for a glass fiber solution to reconstruct or repair parts made from plain weave or twill fiber with about 0,3mm thickness. 
I wil not have access to vacuum, so it will be akin to skinning the affected zone. I'm not dealing with structural parts.
This product seems to meet the requirements 280g 2x2 Twill Woven Glass 1000mm Wide.

Thank you.