By Zapan - 7/29/2020 2:09:55 PM
Hello.
Im looking for a glass fiber solution to reconstruct or repair parts made from plain weave or twill fiber with about 0,3mm thickness. I wil not have access to vacuum, so it will be akin to skinning the affected zone. I'm not dealing with structural parts. This product seems to meet the requirements 280g 2x2 Twill Woven Glass 1000mm Wide.
Thank you.
|
By Warren (Staff) - 7/29/2020 2:46:49 PM
Our 280g 2x2 Twill Woven Glass can be used for fibreglass repairs no problem. It is around 0.3mm thick and being twill weave, is still able to be draped around curves without difficulty. So you should be able to build up your repair patch fairly easily.
|
|