Hello.

Im looking for a glass fiber solution to reconstruct or repair parts made from plain weave or twill fiber with about 0,3mm thickness. 
I wil not have access to vacuum, so it will be akin to skinning the affected zone. I'm not dealing with structural parts.
This product seems to meet the requirements 280g 2x2 Twill Woven Glass 1000mm Wide.

Thank you.



Warren (Staff)
Warren (Staff)
Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
Our 280g 2x2 Twill Woven Glass can be used for fibreglass repairs no problem. It is around 0.3mm thick and being twill weave, is still able to be draped around curves without difficulty.  So you should be able to build up your repair patch fairly easily. 

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search