Hi J
I assume what your doing in vacuum bagging and not infusion. In wet layup vaccum bagging you aren't removing any resin from the bag ,you are just moving it around.
With full vac you will be fine, you are squeezing the stack with full atmospheric pressure so only the excess resin will flow through your perferated film into the bleeder cloth. Full vac will give you a much denser stronger part.
Hope this helps.