Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Advanced Composites Forum
»
Hand Layup
»
what vacuum pressures with breadrap and perforated release film
what vacuum pressures with breadrap and perforated release film
Post Reply
Like
3
what vacuum pressures with breadrap and perforated release film
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
Jcookson
Jcookson
posted 13 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 5,
Visits: 124
just wondering what pressures i should be using with bread rap after hand laying and vac bagging and what pressure to use with the perfortated film as the bread rap has alotmore holes more resin can be pulled out and theres a risk of a dry laminate.
can i vac at full pressure with the perforated release film aswel.
thanks
Reply
Like
3
Reply
Matthieu Libeert
Matthieu Libeert
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 955,
Visits: 3.4K
No did it before and didn't have any problems... can be different from resin to resin maybe... dont know
Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
what vacuum pressures with breadrap and perforated release film
Jcookson
-
13 Years Ago
curious what other forum-members will tell, I always did full vacuum with setup: Carbon - Peelply -...
matthieutje65
-
13 Years Ago
[quote][b]matthieutje65 (06/12/2012)[/b][hr]curious what other forum-members will tell, I always did...
fgayford
-
13 Years Ago
[quote][b]fgayford (16/12/2012)[/b][hr][quote][b]matthieutje65 (06/12/2012)[/b][hr]curious what...
matthieutje65
-
13 Years Ago
What about with bread rap though?
Jcookson
-
13 Years Ago
Hi J I assume what your doing in vacuum bagging and not infusion. Inwet layup vaccum bagging you...
fgayford
-
13 Years Ago
With epoxy I always use full vac for wet lay, highest I can go for polyester is .81
ajb100
-
13 Years Ago
I was told that one should not vac bag polyester parts because it will suck the styrene out of the...
Leew
-
12 Years Ago
No did it before and didn't have any problems... can be different from resin to resin maybe... dont...
matthieutje65
-
12 Years Ago
What can happen with polyester is the decrease pressure can cause the styrene to boil but infusion...
ajb100
-
12 Years Ago
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search