Mould Making Starter Kit


Author
Message
Jack.Strong
Jack.Strong
Supreme Being (356 reputation)Supreme Being (356 reputation)Supreme Being (356 reputation)Supreme Being (356 reputation)Supreme Being (356 reputation)Supreme Being (356 reputation)Supreme Being (356 reputation)Supreme Being (356 reputation)Supreme Being (356 reputation)
Group: Forum Members
Posts: 52, Visits: 549
Here is a photo of the pattern, it has since been painted.



So I will be making a 2 part mould around this pattern. The sheet wax is so I can then use the pattern as a internal mould.
MaxiDave
MaxiDave
Supreme Being (112 reputation)Supreme Being (112 reputation)Supreme Being (112 reputation)Supreme Being (112 reputation)Supreme Being (112 reputation)Supreme Being (112 reputation)Supreme Being (112 reputation)Supreme Being (112 reputation)Supreme Being (112 reputation)
Group: Forum Members
Posts: 14, Visits: 158

Warren
Warren
Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)
Group: Administrators
Posts: 214, Visits: 782
to add to that, how many layers of fibreglass you need depends on the total size and how its supported when fitted.  With what looks like a few bends in it, it may well be fairly stiff with only 3 or 4 layers.  If you curved the edges to have an oblong duct rather than rectangular, it would be even stiffer.
wozza
wozza
Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)
Group: Forum Members
Posts: 688, Visits: 5.4K
Hi I may have misunderstood what you are trying to do but here goes!!!!!

Assuming that the outer lip is just a flange for the mould and not part of the actual duct I don,t understand why you need the sheet wax.
which is the good face, inside or outside of the duct?
If the outside is the "seen" face I would just make a split mould of the "buck" ( I can recommend the EC Uni Mould System)
Lay up the two moulds in CF/GRP.
Bond the two halves together.
Trim off the Flange.

Regards Warren

Carbon Copies Ltd
Jack.Strong
Jack.Strong
Supreme Being (356 reputation)Supreme Being (356 reputation)Supreme Being (356 reputation)Supreme Being (356 reputation)Supreme Being (356 reputation)Supreme Being (356 reputation)Supreme Being (356 reputation)Supreme Being (356 reputation)Supreme Being (356 reputation)
Group: Forum Members
Posts: 52, Visits: 549
It is an aid duct for a car Satisfied

I will try carbon fibre someday but its still a prototype so dont want to waste expensive material.

If I wax and pva why would it stick ? I have come up with a way of holding the pattern 1mm away from the mould but if you think 1mm thickness is too thin then back to the drawing board Tongue
Matthieu Libeert
Matthieu Libeert
Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)
Group: Forum Members
Posts: 955, Visits: 3.4K
Hi, First of all may I ask you what it is? BigGrin

About the 1mm fiberglass, sounds like not much, I would personaly make it a bit thicker (just intuition)

About the mouldmaking kit, I cant help you, never used it before... maybe someone else can help you.

I hope you know that the pattern will be stuck then when finnished? unless you have a solution for that? Smile

Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com




Jack.Strong
Jack.Strong
Supreme Being (356 reputation)Supreme Being (356 reputation)Supreme Being (356 reputation)Supreme Being (356 reputation)Supreme Being (356 reputation)Supreme Being (356 reputation)Supreme Being (356 reputation)Supreme Being (356 reputation)Supreme Being (356 reputation)
Group: Forum Members
Posts: 52, Visits: 549
Hi,



After lots of planning I am about to commit to my project and buy some mould making materials. As you can see from the simple cad, I will be making a 2 part mould, however I intend on using the pattern as an internal mould. So will be applying a layer of sheet wax onto the pattern first. 

I have a few questions:

I intend to make the final part out of fibreglass, would a thickness of 1mm, including top coat be enough for a rigid part ?

I will be buying the "Epoxy Mould Making Starter Kit". Is there enough to make moulds of both sides ? The front face length is 280mm

more to follow.

Thanks