Hi,



After lots of planning I am about to commit to my project and buy some mould making materials. As you can see from the simple cad, I will be making a 2 part mould, however I intend on using the pattern as an internal mould. So will be applying a layer of sheet wax onto the pattern first. 

I have a few questions:

I intend to make the final part out of fibreglass, would a thickness of 1mm, including top coat be enough for a rigid part ?

I will be buying the "Epoxy Mould Making Starter Kit". Is there enough to make moulds of both sides ? The front face length is 280mm

more to follow.

Thanks
Reply
Jack.Strong
Jack.Strong
Supreme Being (354 reputation)Supreme Being (354 reputation)Supreme Being (354 reputation)Supreme Being (354 reputation)Supreme Being (354 reputation)Supreme Being (354 reputation)Supreme Being (354 reputation)Supreme Being (354 reputation)Supreme Being (354 reputation)
Group: Forum Members
Posts: 52, Visits: 549
Here is a photo of the pattern, it has since been painted.



So I will be making a 2 part mould around this pattern. The sheet wax is so I can then use the pattern as a internal mould.