Hello,

I'm  a newbie  to the forum and but I hope that someone here can help me.
I,m  using Xencast P2 for casting and have problem with bubbles forming on the surface of the cast. Can I use slightly less hardner in the mix to extend the pot life of the resin and allow more time for the air bubbles to escape?