By szmn - 2/21/2020 2:53:02 PM
Hello,
I'm a newbie to the forum and but I hope that someone here can help me. I,m using Xencast P2 for casting and have problem with bubbles forming on the surface of the cast. Can I use slightly less hardner in the mix to extend the pot life of the resin and allow more time for the air bubbles to escape?
|
By szmn - 2/28/2020 11:30:35 AM
Thanks for the reply. I will try the whipping technique then.
|
|