The only problem with the PX90 is it is not 100% UV stable so if exposed to direct sunlight all the time it would eventually degrade. If it is between the collar and mast and effectively protected then this might not be an issue.
Warren Penalver Easy Composites / Carbon Mods - Technical Support Assistant
|