By aran01 - 2/9/2020 10:02:39 AM
Hi folks, My boat mast which sits on the deck had very unsightly bits of rubber around it to fill the gap between the mast and the collar. See pictures. This time around I am considering pouring some XenCast PX90 into the gap when the mast is stepped, having first applied PVA to the mast and the collar. Do you think this is the best course of action or is there a better / other product I could use? Thanks, Micheal
|
By Warren (Staff) - 2/19/2020 2:36:14 PM
PVA mould release would certainly help, as would any release agent.
|
|