carbon fibre matt finish


Author
Message
Mitch
M
Forum Member (45 reputation)Forum Member (45 reputation)Forum Member (45 reputation)Forum Member (45 reputation)Forum Member (45 reputation)Forum Member (45 reputation)Forum Member (45 reputation)Forum Member (45 reputation)Forum Member (45 reputation)
Group: Forum Members
Posts: 3, Visits: 17
Hi guys, newbie here.

I would like to have a matte carbon finish, but i really don't find this much information online and i thought i might as well ask the pro's on this forum what would be the best coarse of action.

1)  Wet sand it with  400-800, (1200?) done

or

2) wet sand it with  400'ish grid and then spray a matte lacquer on there (if so what lacquer would u use, a car lacquer or just a normal lacquer for wood, metal, plastic purposes?)
=> would this one do Motip acryl matte lacquer?


thanks in advance Mitch