Group: Forum Members
Posts: 3,
Visits: 17
|
Hi guys, newbie here.
I would like to have a matte carbon finish, but i really don't find this much information online and i thought i might as well ask the pro's on this forum what would be the best coarse of action.
1) Wet sand it with 400-800, (1200?) done
or
2) wet sand it with 400'ish grid and then spray a matte lacquer on there (if so what lacquer would u use, a car lacquer or just a normal lacquer for wood, metal, plastic purposes?) => would this one do Motip acryl matte lacquer?
thanks in advance Mitch
|