Group: Forum Members
Posts: 408,
Visits: 4.1K
|
I have used standard window glass. Even used old double glazed units (but remember to drill a few holes in the material holding the two pieces together so the expanding air can escape!
I have also used mirrors, as these are very flat.
I have had no issues up to 140 deg C using a 3 deg C per minute ramp cycle.
|