Pre-preg sheets what type of glass is need to deal with oven temps etc


Pre-preg sheets what type of glass is need to deal with oven temps etc
Author
Message
ally0640
a
Junior Member (18 reputation)Junior Member (18 reputation)Junior Member (18 reputation)Junior Member (18 reputation)Junior Member (18 reputation)Junior Member (18 reputation)Junior Member (18 reputation)Junior Member (18 reputation)Junior Member (18 reputation)
Group: Forum Members
Posts: 1, Visits: 7
I need to make some pre preg sheets from a sheet of glass but type of glass should i use ?
Lester Populaire
L
Supreme Being (4.3K reputation)Supreme Being (4.3K reputation)Supreme Being (4.3K reputation)Supreme Being (4.3K reputation)Supreme Being (4.3K reputation)Supreme Being (4.3K reputation)Supreme Being (4.3K reputation)Supreme Being (4.3K reputation)Supreme Being (4.3K reputation)
Group: Forum Members
Posts: 311, Visits: 13K
ally0640 - 1/4/2020 5:33:30 PM
I need to make some pre preg sheets from a sheet of glass but type of glass should i use ?

I use tempered safety glass with 8mm thickness. Never had an issue with that, but never tried anything else either. Not very demanding application tho as with the slow ramp rates you will have very uniform temperatures within the glass. However, i think tempered glass is a smart choice nevertheless. 

Steve Broad
Steve Broad
Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)
Group: Forum Members
Posts: 408, Visits: 4.1K
I have used standard window glass. Even used old double glazed units (but remember to drill a few holes in the material holding the two pieces together so the expanding air can escape!

I have also used mirrors, as these are very flat.

I have had no issues up to 140 deg C using a 3 deg C per minute ramp cycle.