Just trying to debulk my layup but I seem to be having issues with the silicone connector.  The connector draws a partial vacuum down to -0.5bar and then stops. It hisses a lot.  I have tried several times to get a vacuum, with copious amounts of gum tape etc, but just cannot get a full vacuum.  Anyone seen this before?